Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 56.00 °C | 132.8 °F | ASTM D-648 |
Axiall 9175 Amber 12 Rigid PVC, Molding, Amber 12 Georgia Gulf 9175 Amber 12 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It is a pre-colored amber compound.Information provided .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.00 °C | 132.8 °F | ASTM D-648 |
Axiall 9275J Clear 38 Rigid PVC, Molding, Clear 38 Georgia Gulf 9275J Clear 38 is a food grade used for injection blow molded packages in critical medical, cosmetic and toiletry applications. All ingredients are FDA approved.Information provided by.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 56.00 °C | 132.8 °F | ASTM D-648 |
Axiall 9175J Clear 38 Rigid PVC, Molding, Clear 38 Georgia Gulf 9175J Clear 38 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It has excellent clarity, flow and stability.Informatio.. |