Deflection Temperature at 1.8 MPa (264 psi) 120.5 °C
248.9 °F
unannealed; ASTM D648
KYDEX® FST Fully Compliant Aviation Thermoforming Sheet
KYDEX® FST meets all fire, smoke and heat release requirements set forth by the Federal Aviation Regulations 25.853 paragraphs (a) and (d) as well as toxicity requirements for ABD0031, BSS7239 an..