KYDEX® FST Fully Compliant Aviation Thermoforming Sheet

Category Polymer , Thermoplastic
Manufacturer KYDEX LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KYDEX® FST Fully Compliant Aviation Thermoforming Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KYDEX® FST meets all fire, smoke and heat release requirements set forth by the Federal Aviation Regulations 25.853 paragraphs (a) and (d) as well as toxicity requirements for ABD0031, BSS7239 and D6-51377.Suggested Applications:Seat partsBulkhead laminatesLife vest shroudsPassenger service unitsMonitor shroudsArmrestsWindow shadesMolding stripsTray tablesKick panelsInformation provided by Kydex, LLC.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 125
125
ASTM D785
Tensile Strength 74.0 MPa
10700 psi
ASTM D638
Flexural Strength 107 MPa
15500 psi
ASTM D790
Flexural Modulus 2.32 GPa
336 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 120.5 °C
248.9 °F
unannealed; ASTM D648
Descriptive Properties Value Comments
Federal Aviation Administration < 65/65
FAR 25.853 (d); Rate of Heat Release
Pass
FAR 25.853 (a)
Pass
FAR 25.853 (d); Smoke Generation
Toxicity Requirements ABD0031
Pass
BSS 7239
Pass
D6-51377
Pass