Thermal Properties | Metric | English | Comments |
---|---|---|---|
Beta Transus | 895 °C | 1640 °F | |
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); STA Cold Formable Medium-Strength AlloyFeatures: This binary, age hardening alloy combines the easy formability and weldability of commercially pure titanium with improved mechanical properties, particu.. |
|||
Beta Transus | 895 °C | 1640 °F | |
TIMET TIMETAL® 230 Titanium Alloy (Ti-2.5Cu); Annealed Cold Formable Medium-Strength AlloyIndustry Specifications: Germany Aerospace: 3.7124. France: T-U2. UK Aerospace Specifications BA TA. 21, 22, 23.Features: This binary, age hardening alloy combi.. |