Polymer Property : Deflection Temperature at 8.0 MPa = 446 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 230 °C
446 °F
ISO 75-1/-2
EMS-Grivory Grivory® HT2V-5H PA6T/66-GF50
Product description: Grivory HT2V-5H is a 50 % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO:..
Deflection Temperature at 8.0 MPa 230 °C
446 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSGL-50-4 black 9839 PA666-GF50
Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following ..
Deflection Temperature at 8.0 MPa 230 °C
446 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSGL-50-4 nat PA666-GF50
Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following ..
Deflection Temperature at 8.0 MPa 230 °C
446 °F
ISO 75-1/-2
EMS-Grivory Grivory® GV XE 16102 (GVL-6H HP) PA*-GF60
Product description: Grivory XE 16102 natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long special glass fibers. Grivory..
Deflection Temperature at 8.0 MPa 230 °C
446 °F
HDT/C; ISO 75-2
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..