Material Notes:
Product description: Grilon TSGL-50/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 natural is characterized by the following key-properties: high stiffness and strength even after conditioning and over a wide temperature rangeexcellent notched impact resistance also at low temperatureslow creephigh heat distortion temperaturesgood dimensional stability and little warpagegood surface appearance and ease of processing The product has been designed for injection molding of technical parts especially in the area of die-cast metal replacement. Grilon TSGL-50/4 natural is used in the following market segments: automotivemechanical engineeringhousehold and appliances The glass-fibers are aligned in parallel and are just as long as the pellets (usually 10 mm).Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183
Water Absorption 4.5 %
4.5 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
0.0030 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Ball Indentation Hardness 200 MPa
29000 psi
conditioned; ISO 2039-1
310 MPa
45000 psi
dry; ISO 2039-1
Tensile Strength at Break 200 MPa
29000 psi
conditioned; ISO 527-1/-2
260 MPa
37700 psi
dry; ISO 527-1/-2
Elongation at Break 2.3 %
2.3 %
dry; ISO 527-1/-2
2.5 %
2.5 %
conditioned; ISO 527-1/-2
Tensile Modulus 12.5 GPa
1810 ksi
conditioned; ISO 527-1/-2
17.5 GPa
2540 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 10.0 J/cm²
47.6 ft-lb/in²
dry; ISO 179/1eU
10.5 J/cm²
50.0 ft-lb/in²
conditioned; ISO 179/1eU
7.50 J/cm²

@Temperature 30.0 °C
35.7 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
9.50 J/cm²

@Temperature 30.0 °C
45.2 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
Charpy Impact, Notched 4.00 J/cm²
19.0 ft-lb/in²
dry; ISO 179/1eA
4.50 J/cm²
21.4 ft-lb/in²
conditioned; ISO 179/1eA
4.00 J/cm²

@Temperature 30.0 °C
19.0 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
4.50 J/cm²

@Temperature 30.0 °C
21.4 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
11.1 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
27.8 µin/in-°F
ISO 11359-1/-2
Melting Point 260 °C
500 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 120 - 130 °C
248 - 266 °F
long term; EMS
220 °C
428 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 230 °C
446 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
1.00e+13 ohm-cm
1.00e+13 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Strength 24.0 kV/mm
610 kV/in
conditioned; IEC 60243-1
29.0 kV/mm
737 kV/in
dry; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Cooling and climate control
Exterior
Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Energy distribution
Form Granules
Industry & Consumer goods Housewares
Hydraulics & Pneumatics
Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Improved flowability and demoulding
Long Fiber Reinforced
Special Characteristics Improved heat resistance