Thermal Properties Metric English Comments
Glow Wire Test 600 °C

@Thickness 2.00 mm
1110 °F

@Thickness 0.0787 in
GWFI; IEC 60695-2-12
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber
SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme..