Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= 70.0 °C | <= 158 °F | ISO 974 |
DuPont Performance Polymers Hytrel® HTR8241 TPC-ET
(Unverified Data**) Hytrel® HTR8241 is a 65 nom.Shore D, non discoloring stabilizer, plasticiser free high performance resin for extrusion; high viscosity; outstanding mechanical properties up to 120°C and excellent .. |