Thermal Properties Metric English Comments
Brittleness Temperature <= 70.0 °C
<= 158 °F
ISO 974
DuPont Performance Polymers Hytrel® HTR8241 TPC-ET  (Unverified Data**)
Hytrel® HTR8241 is a 65 nom.Shore D, non discoloring stabilizer, plasticiser free high performance resin for extrusion; high viscosity; outstanding mechanical properties up to 120°C and excellent ..