Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -30.0 - 15.0 °C | -22.0 - 59.0 °F | Average value: -13.1 °C Grade Count:8 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Brittleness Temperature | -80.0 - 15.0 °C | -112 - 59.0 °F | Average value: -29.9 °C Grade Count:784 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |