Thermal Properties Metric English Comments
Brittleness Temperature -30.0 - 15.0 °C
-22.0 - 59.0 °F
Average value: -13.1 °C Grade Count:8
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Brittleness Temperature -80.0 - 15.0 °C
-112 - 59.0 °F
Average value: -29.9 °C Grade Count:784
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..