Polymer Property : Brittleness Temperature = -90.6 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature <= -90.6 °C
<= -131 °F
ASTM D746
Amco PRIMATOP HDPE HMW 1000950 High Molecular Weight Copolymer
HDPE HMW 1000950 features good melt strength, excellent stress cracking resistance, good rigidity, and excellent impact strength. Applications include agricultural chemical tanks, pallets, and large..
Brittleness Temperature <= -90.6 °C
<= -131 °F
ASTM D746
Formosa Plastics Formolene® HL5010 Blow Molding HDPE
Extra High Molecular Weight Hexene CopolymerApplications: Blow Molded 55-gallon shipping containers, gasoline tanks, agricultural chemical tanks; Extruded pallets, cattle feeders, large formed parts..