Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -90.6 °C | <= -131 °F | ASTM D746 |
Amco PRIMATOP HDPE HMW 1000950 High Molecular Weight Copolymer HDPE HMW 1000950 features good melt strength, excellent stress cracking resistance, good rigidity, and excellent impact strength. Applications include agricultural chemical tanks, pallets, and large.. |
|||
Brittleness Temperature | <= -90.6 °C | <= -131 °F | ASTM D746 |
Formosa Plastics Formolene® HL5010 Blow Molding HDPE Extra High Molecular Weight Hexene CopolymerApplications: Blow Molded 55-gallon shipping containers, gasoline tanks, agricultural chemical tanks; Extruded pallets, cattle feeders, large formed parts.. |