Thermal Properties Metric English Comments
Brittleness Temperature -54.0 °C
-65.2 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable W1250L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Brittleness Temperature -54.0 °C
-65.2 °F
Momentive Performance Materials RTV31 Silicone Rubber Compound for High Temperature, Red
RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa..
Brittleness Temperature -54.0 °C
-65.2 °F
Momentive Performance Materials RTV88 Silicone Rubber Compound for High Temperature, Red
RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa..
Brittleness Temperature -54.0 °C
-65.2 °F
Momentive Performance Materials RTV60 Silicone Rubber Compound for High Temperature, Red
RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa..
Brittleness Temperature -54.0 °C
-65.2 °F
ASTM D746
Teknor Apex Flexalloy® 9800-40 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and ..
Brittleness Temperature -54.0 °C
-65.2 °F
ASTM D746
Teknor Apex Flexalloy® 9900-40 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and ..
Brittleness Temperature -54.0 °C
-65.2 °F
ASTM D746
Teknor Apex Flexalloy® 9900-45 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and ..
Brittleness Temperature -54.0 °C
-65.2 °F
Type A, type 1 specimen; ASTM D746
Chevron Phillips Marlex® 1009 LDPE Injection Molding Resin
Resin Type: HomopolymerCharacteristics: Excellent flexibilityExcellent flowModerate mold releaseGood warpage resistanceApplications: Large housewaresTamper evident, snap-on capsFeminine hygiene appl..
Brittleness Temperature -54.0 °C
-65.2 °F
XT<sub>b</sub>; ASTM D746
Colorite Polymers Elastichem 6011TX-02 Vinyl Compound
Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co..
Brittleness Temperature -54.0 °C
-65.2 °F
ASTM D2137
Aearo E-A-R Specialty Composites VersaDamp™ V-2550 TPE
VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded..
Brittleness Temperature -54.0 °C
-65.2 °F
ASTM D746
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer
Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Brittleness Temperature -54.0 °C
-65.2 °F
ASTM D-746
Axiall 8730 Moldings & Extrusions Flexible PVC
A high quality, profile extrusion compound recommended for those applications where exceptional low temperature performance is required.Information provided by Georgia GulfGeorgia Gulf became Axiall..
Brittleness Temperature -54.0 °C
-65.2 °F
ASTM D746
PolyOne Synprene® RT-5165 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalIgnition ResistantApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Injection Mo..