Chevron Phillips Marlex® 1009 LDPE Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® 1009 LDPE Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Type: HomopolymerCharacteristics: Excellent flexibilityExcellent flowModerate mold releaseGood warpage resistanceApplications: Large housewaresTamper evident, snap-on capsFeminine hygiene applicationsInformation provided by Chevron Phillips.
Physical Properties Metric English Comments
Density 0.917 g/cc
0.0331 lb/in³
ASTM D1505
Melt Index of Compound 16 g/10 min
16 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 46
46
ASTM D2240
Tensile Strength, Yield 9.00 MPa
1310 psi
2 in/min, Type IV bar; ASTM D638
Elongation at Break 500 %
500 %
2 in/min, Type IV bar; ASTM D638
Flexural Modulus 0.200 GPa
29.0 ksi
Tangent, 16:1 span:depth,0.5in/min; ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 85.0 °C
185 °F
Loading 1, Rate A; ASTM D1525
Brittleness Temperature -54.0 °C
-65.2 °F
Type A, type 1 specimen; ASTM D746