Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -73.0 - -65.0 °C | -99.4 - -85.0 °F | Average value: -70.3 °C Grade Count:3 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |