Thermal Properties Metric English Comments
Brittleness Temperature -32.8 °C
-27.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible A8500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Brittleness Temperature -32.8 °C
-27.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible A8501 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Brittleness Temperature -32.8 °C
-27.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible A8504 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -32.8 °C
-27.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible A85UB Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -32.8 °C
-27.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible G8024 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -32.8 °C
-27.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible R336AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne