Brittleness Temperature -76.1 - -27.0 °C
-105 - -16.6 °F
Average value: -68.0 °C Grade Count:32
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..
Brittleness Temperature -90.0 - -27.0 °C
-130 - -16.6 °F
Average value: -62.1 °C Grade Count:31
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and ..