Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -21.7 °C | -7.06 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible D75M0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -21.7 °C | -7.06 °F | ASTM D746 |