PolyOne Geon™ Vinyl Flexible B80MB Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible B80MB Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.011 - 0.015 cm/cm
0.011 - 0.015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
15 sec; ASTM D2240
80
80
ASTM D2240
Tensile Strength at Break 15.2 MPa
2200 psi
510 mm/min; ASTM D638
Tensile Strength 6.89 MPa

@Strain 100 %
999 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 420 %
420 %
510 mm/min; ASTM D638
Tear Strength 48.2 kN/m
275 pli
Die C, 510 mm/min; ASTM D624
Compression Set 55 %

@Temperature 23.0 °C,
Time 79200 sec
55 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -21.7 °C
-7.06 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 174 - 179 °C
345 - 354 °F
191 - 202 °C
376 - 396 °F
Descriptive Properties Value Comments
Additive Biocide
Features General Purpose
Low to No Migration
Medium Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses General Purpose