Thermal Properties Metric English Comments
Brittleness Temperature -126 °C
-195 °F
ASTM D746
Ashley Polymers Ashlene® 980LS Nylon 612
A general purpose 612 nylon for injection molding, lubricated and heat stabilized. These resins are noted for their low moisture absorption and excellent dimensional stability.Data provided by the ..
Brittleness Temperature -126 °C
-195 °F
ASTM D746
Ashley Polymers Ashlene® 981S Nylon 612
A general purpose heat stabilized 612 Nylon for extrusion. These resins are noted for their low moisture absorption and excellent dimensional stability.Data provided by the manufacturer