Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -126 °C | -195 °F | ASTM D746 |
Ashley Polymers Ashlene® 980LS Nylon 612 A general purpose 612 nylon for injection molding, lubricated and heat stabilized. These resins are noted for their low moisture absorption and excellent dimensional stability.Data provided by the .. |
|||
Brittleness Temperature | -126 °C | -195 °F | ASTM D746 |
Ashley Polymers Ashlene® 981S Nylon 612 A general purpose heat stabilized 612 Nylon for extrusion. These resins are noted for their low moisture absorption and excellent dimensional stability.Data provided by the manufacturer |