Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -91.0 °C | <= -132 °F | ASTM D746 |
Chevron Phillips Marlex® HXM 50100-02 Extra high molecular weight hexene copolymer
(discontinued **) Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesCharacteristics:.. |
|||
Brittleness Temperature | <= -91.0 °C | <= -132 °F | ASTM D746 |
Formosa Plastics Formolene® HL5010 Sheet and Thermoforming HDPE
(discontinued **) Extra High Molecular Weight Hexene Copolymer Formolene® HL5010 has good melt strength, excellent stress crack resistance, good rigidity, and excellent impact strength even at low temperatures. Thes.. |
|||
Brittleness Temperature | <= -91.0 °C | <= -132 °F | ASTM D746 |
Chevron Phillips Marlex® HXM 50100 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Brittleness Temperature | <= -91.0 °C | <= -132 °F | ASTM D746 |
Chevron Phillips Marlex® HXM 50100-01 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
Brittleness Temperature | -91.1 °C | -132 °F | ASTM D746; ISO 812 |
Advanced Polymer Alloys Alcryn® 2250 UT Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Brittleness Temperature | -91.1 °C | -132 °F | ASTM D746; ISO 812 |
Advanced Polymer Alloys Alcryn® 2265 UT Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |