Thermal Properties Metric English Comments
Brittleness Temperature <= -83.0 °C
<= -117 °F
ASTM D746
Dow AMPLIFY™ EA 103 Ethylene-ethyl Acrylate (EEA)
AMPLIFY™ EA 103 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. It can be ut..