Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 3.00 mm |
140 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources ABS-GP1-[color]-UV General Purpose ABS, UV-stabilized General Purpose Acrylonitrile Butadiene Styrene, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.In.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness 1.50 mm |
140 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC/ABS-FR2 Flame Retardant PC/ABS Alloy, High Flow PC/ABS Alloy, Flame Retardant, Higher FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical AF342 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=2.50 mm |
140 °F @Thickness >=0.0984 in |
|
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=2.50 mm |
140 °F @Thickness >=0.0984 in |
|
LG Chemical AF345 ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided by LG Chemi.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical HF380NS ABS, High Flow, General Anti-Static Feature: Injection Molding, High Flow, General Anti-StaticApplication: Electric & Electronic Products, Miscellaneous goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical HG173 ABS, High Surface Gloss Feature: Injection Molding, High Surface GlossApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical LUMAX GP5306F PBT+ABS+GF30%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF30%, Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4Information provided by LG .. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.20 mm |
140 °F @Thickness >=0.0472 in |
|
LG Chemical LUPOY GN5001RFH PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat ResistanceApplication: E&E (TV, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Ch.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=2.00 mm |
140 °F @Thickness >=0.0787 in |
|
LG Chemical LUPOY GN5008HF PC/ABS, Halogen Free Flame Retardant, High Impact Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: E&E (OA, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN5008HF PC/ABS, Halogen Free Flame Retardant, High Impact Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: E&E (OA, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.00 mm |
140 °F @Thickness >=0.0394 in |
|
LG Chemical LUPOY GN5008HF PC/ABS, Halogen Free Flame Retardant, High Impact Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: E&E (OA, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.60 mm |
140 °F @Thickness >=0.0630 in |
|
LG Chemical LUPOY HR5007A PC/ABS, Heat Resistance, High Impact Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High Impact.Application: Automotive (Interior), E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY HR5007AE PC/ABS, High Impact Description: Injection Molding, PC/ABS, High Flow, High ImpactApplication: E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY MP5000AM PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Metal PlatingApplication: Automotive (Exterior), E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical PT270 ABS Feature: Injection Molding, Good PaintabilityApplication: Exterior Part of Automobile and Motor cycleCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.20 mm |
140 °F @Thickness >=0.0472 in |
|
LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
|
LG Chemical LUPOY GN5009F PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
|
LG Chemical LUPOY GN5101RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=3.00 mm |
140 °F @Thickness >=0.118 in |
UL 746B |
LG Chemical XR407D ABS Feature: Electric & Electronic HousingApplication: Electric & Electronic HousingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=1.50 mm |
140 °F @Thickness >=0.0591 in |
UL 746B |
LG Chemical SG175G ABS, Super Surface Gloss, High Flow Feature: Injection Molding, Super Surface Gloss, High FlowApplication: Electric & Electronic ProductsCAS No. 9003-56-9Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 60.0 °C @Thickness >=2.00 mm |
140 °F @Thickness >=0.0787 in |
|
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS+GF20%, Halogen Free Flame Retardant, High StiffnessApplication: E&E (Housing, OA Frame)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 65997-17-3Information provi.. |