Polymer Property : UL RTI, Electrical = 310 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Electrical 154 °C

@Thickness 3.00 mm
310 °F

@Thickness 0.118 in
UL 746
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow
Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/..
UL RTI, Electrical 154 °C

@Thickness 3.00 mm
310 °F

@Thickness 0.118 in
UL 746
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release
Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform..