Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 154 °C @Thickness 3.00 mm |
310 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
UL RTI, Electrical | 154 °C @Thickness 3.00 mm |
310 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |