Polymer Property : Glow Wire Test = 930 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glow Wire Test 930 °C
1710 °F
IEC 60695-2-13
SABIC Innovative Plastics EXTEM UH1006 TPI Blend
High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha..
Glow Wire Test 930 °C
1710 °F
IEC 60695-2-13
SABIC Innovative Plastics EXTEM UH1026 TPI Blend
High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent