Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -7.00 °C | 19.4 °F | Base Oil; ASTM D97 |
Nye Lubricants 100 (DMO) Delicate Machinery Oil Information provided by Nye Lubricants. |
|||
Pour Point | -7.00 °C | 19.4 °F | |
ChevronTexaco 100 Honor Ashless AW Texaco Honor Ashless AW are circulating oils formulated from high quality base stocks and a carefully balanced, zinc-free additive package. These proved excellent protection against wear for long be.. |
|||
Pour Point | -7.00 °C | 19.4 °F | |
ChevronTexaco 460 Honor Ashless AW Texaco Honor Ashless AW are circulating oils formulated from high quality base stocks and a carefully balanced, zinc-free additive package. These proved excellent protection against wear for long be.. |
|||
Pour Point | -7.00 °C | 19.4 °F | ASTM D97 |
ChevronTexaco Superla® 5 White Oil FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F.These nearly ch.. |
|||
Pour Point | -7.00 °C | 19.4 °F | |
ExxonMobil Mobil Vaprotec Light Mobil Vaprotec Light is an ISO Viscosity Grade 32, turbine-quality circulation oil containing anti-oxidants and defoamants. It is enhanced with a three-phase rust inhibitor to protect surfaces light.. |
|||
Pour Point | -7.00 - -1.00 °C | 19.4 - 30.2 °F | |
Solvay RHODASURF® BC-630 Surfactant Chemical Name: TRIDECYL ALCOHOL ETHOXYLATEDCAS: 78330-21-9 (Generic)Available in: Asia Pacific, Europe, Latin America and North America Solubility: Insoluble in water, dispersible in alcohol, minera.. |
|||
Pour Point | -7.00 °C | 19.4 °F | |
ExxonMobil Mobil Vaprotec Light Mobil Vaprotec Light is an ISO Viscosity Grade 32, turbine-quality circulation oil containing anti-oxidants and defoamants. It is enhanced with a three-phase rust inhibitor to protect surfaces light.. |