Pour Point -23.0 °C
-9.40 °F
Base Oil; ASTM D97
Nye Lubricants 730F (NG) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -23.0 °C
-9.40 °F
Base Oil; ASTM D97
Nye Lubricants 760W (NG) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -23.0 °C
-9.40 °F
ASTM D97
Solvay Specialty Polymers FOMBLIN® Y H-VAC 140/13 PFPE Pump Oil
FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and..
Pour Point -23.0 °C
-9.40 °F
ASTM D97
ExxonMobil 120 Exxon Aviation Oil EE Series
Aviation Oil EE is the brand name of a premium quality line of ashless-dispersant piston engine oils. Formulated with select, highly refined base oils together with ashless-dispersant and anti-oxida..
Pour Point -23.0 °C
-9.40 °F
ASTM D97
ChevronTexaco 100 NC Open Gear Lubricant
FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri..
Pour Point -23.0 °C
-9.40 °F
ChevronTexaco L Metal Protective Oil L
Texaco Metal Protective Oil L delivers value through:Excellent short-term rust protection — After evaporation of the solvent, a highly protective, nondrying oil film remains which provides a higher..
Pour Point -23.0 °C
-9.40 °F
ASTM D97
ExxonMobil 120 Exxon Aviation Oil EE Series