Category Fluid , Lubricant , Perfluoropolyether (PFPE)
Manufacturer Solvay Specialty Polymers (former Solexis)
Trade Name FOMBLIN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers FOMBLIN® Y H-VAC 140/13 PFPE Pump Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and oxygen atoms, the PFPEs have exceptional properties such as: low vapor pressure; chemical inertness; non-flammability; high thermal stability; no flash or fire point; low toxicity; excellent compatibility with metals, plastics, elastomers; low volatility; good aqueous and non-aqueous solvent resistance; high dielectric properties; low surface tension; good radiation stability; and environmentally friendly-do not damage the ozone.Information provided by Solvay Solexis, Inc.
Physical Properties Metric English Comments
Density 1.92 g/cc
0.0694 lb/in³
ASTM D891
Kinematic Viscosity 1508 cSt

@Temperature 20.0 °C
1508 cSt

@Temperature 68.0 °F
ASTM D445
Molecular Weight 6600 g/mol
6600 g/mol
Vapor Pressure 6.70e-16 bar

@Temperature 20.0 °C
5.00e-13 torr

@Temperature 68.0 °F
Knudsen
6.67e-11 bar

@Temperature 100 °C
5.00e-8 torr

@Temperature 212 °F
Knudsen
Thermal Properties Metric English Comments
Heat of Vaporization 20.9 J/g

@Temperature 200 °C
9.00 BTU/lb

@Temperature 392 °F
Pour Point -23.0 °C
-9.40 °F
ASTM D97
Optical Properties Metric English Comments
Refractive Index 1.304
1.304
n<sub>0</sub><sup>20</sup>