Thermal Properties Metric English Comments
Pour Point -90.0 °C
-130 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8950 (497) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -90.0 °C
-130 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8951 (897-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -90.0 °C
-130 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8951R (897RP-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -90.0 °C
-130 °F
Base Oil; ASTM D97
Nye Lubricants UniFlor 8955 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Pour Point -90.0 °C
-130 °F
ASTM D97
Solvay Specialty Polymers FOMBLIN® Z03 PFPE Lubricant
FOMBLIN® Z is a linear PFPE available as a neutral or functionalized fluid. They are used in aerospace, magnetic media, and polymer modification uses.Information provided by Solvay Solexis, Inc...
Pour Point -90.0 °C
-130 °F
3M Fluorinert™ FC-72 Electronic Liquid
3M™ Fluorinert™ Liquid FC-72 is a non-conductive, thermally and chemically stable liquid ideal for many direct contact single and two phase low temperature heat transfer applications, in testing, ..