Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -74.0 °C | -101 °F | |
ChevronTexaco Hydraulic Safety Fluid Texaco Hydraulic Safety Fluid is a fire-resistant fluid designed for use in high pressure hydraulic systems where the requirements for fire resistance, pump wear protection and viscosity are satisfi.. |