Thermal Properties Metric English Comments
UL RTI, Mechanical without Impact 130 - 180 °C
266 - 356 °F
Average value: 137 °C Grade Count:7
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..