UL RTI, Mechanical without Impact 130 - 240 °C
266 - 464 °F
Average value: 199 °C Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..