Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 190 °C

@Thickness 1.57 mm
374 °F

@Thickness 0.0618 in
Solvay Specialty Polymers Veradel® AG-230 Polyethersulfone  (discontinued **)
For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N..