Polymer Property : UL RTI, Mechanical with Impact = 170 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 130 - 170 °C
266 - 338 °F
Average value: 136 °C Grade Count:7
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..