Thermal Properties Metric English Comments
UL RTI, Electrical 240 °C
464 °F
UL 746B
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c..
UL RTI, Electrical 240 °C
464 °F
UL 746B
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
UL RTI, Electrical 240 °C
464 °F
UL 746B
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
UL RTI, Electrical 240 °C
464 °F
UL 746B
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co..