Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 96.8 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 36.0 °C

@Thickness 3.20 mm
96.8 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 241E Non-Reinforced, Extrusion Grade Ionomer Alloy
DescriptionFormion® FI 241E is a patented non-reinforced, extrusion grade Ionomer alloy. It has bee formulated for high durability, low gloss, and low temperature ductility.ApplicationFormion® FI..
Deflection Temperature at 0.46 MPa (66 psi) 36.0 °C

@Thickness 3.20 mm
96.8 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 241E Non-Reinforced, Extrusion Grade Ionomer Alloy
DescriptionFormion® FI 241E is a patented non-reinforced, extrusion grade Ionomer alloy. It has bee formulated for high durability, low gloss, and low temperature ductility.ApplicationFormion® FI..
Deflection Temperature at 0.46 MPa (66 psi) 36.0 °C

@Thickness 3.20 mm
96.8 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 241E Non-Reinforced, Extrusion Grade Ionomer Alloy
DescriptionFormion® FI 241E is a patented non-reinforced, extrusion grade Ionomer alloy. It has bee formulated for high durability, low gloss, and low temperature ductility.ApplicationFormion® FI..
Deflection Temperature at 0.46 MPa (66 psi) 36.0 °C

@Thickness 3.20 mm
96.8 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 241E Non-Reinforced, Extrusion Grade Ionomer Alloy
DescriptionFormion® FI 241E is a patented non-reinforced, extrusion grade Ionomer alloy. It has bee formulated for high durability, low gloss, and low temperature ductility.ApplicationFormion® FI..
Deflection Temperature at 0.46 MPa (66 psi) 36.0 °C

@Thickness 3.20 mm
96.8 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 241E Non-Reinforced, Extrusion Grade Ionomer Alloy
DescriptionFormion® FI 241E is a patented non-reinforced, extrusion grade Ionomer alloy. It has bee formulated for high durability, low gloss, and low temperature ductility.ApplicationFormion® FI..
Deflection Temperature at 0.46 MPa (66 psi) 36.0 °C

@Thickness 3.20 mm
96.8 °F

@Thickness 0.126 in
ISO 75
A. Schulman FORMION™ FI 241E Non-Reinforced, Extrusion Grade Ionomer Alloy
DescriptionFormion® FI 241E is a patented non-reinforced, extrusion grade Ionomer alloy. It has bee formulated for high durability, low gloss, and low temperature ductility.ApplicationFormion® FI..