DescriptionFormion® FI 241E is a patented non-reinforced, extrusion grade Ionomer alloy. It has bee formulated for high durability, low gloss, and low temperature ductility.ApplicationFormion® FI 241E is targeted for exterior or interior appearance or packaging applications in film, blow molding, thermoforming or extrusion applications, which may require low tack, low gloss, and excellent colorability.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ISO 1183/1
Linear Mold Shrinkage 0.011 - 0.019 cm/cm

@Thickness 3.20 mm
0.011 - 0.019 in/in

@Thickness 0.126 in
72 hr; ISO 294
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
15 sec delay; ISO 868
Tensile Strength, Ultimate 9.50 MPa
1380 psi
at max load; ISO 527
Elongation at Break 165 %
165 %
ISO 527
Flexural Modulus 0.109 GPa
15.8 ksi
Tangent; ISO 178
Izod Impact, Notched (ISO) NB
NB
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 36.0 °C

@Thickness 3.20 mm
96.8 °F

@Thickness 0.126 in
ISO 75