Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 79.4 °C | 175 °F | ASTM D648 |
RheTech Products FT2400-647UV Thermoplastic Polyolefin, UV Stabilized, 8798NM Grey Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 79.4 °C | 175 °F | ASTM D648 |
RheTech Products FT2400-648UV Thermoplastic Polyolefin, UV Stabilized, 848 Black Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 79.4 °C | 175 °F | ASTM D648 |
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 79.4 °C | 175 °F | ASTM D648 |
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 79.4 °C | 175 °F | ASTM D648 |
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 79.4 °C | 175 °F | ASTM D648 |
RheTech Products FT2500-630UV Thermoplastic Polyolefin, UV Stabilized, 500F Light Charcoal Applications: Air DamsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 79.4 °C | 175 °F | ASTM D648 |
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 79.4 °C | 175 °F | ASTM D648 |
Rochling Engineered Plastics Polystone® G HDPE Extruded Sheet Information provided by Röchling Engineered Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 79.4 °C | 175 °F | ASTM D648 |
Global GPP-2000 Polypropylene Impact Copolymer, Cold Temperature Impact Resistant, Nucleated Information provided by Global Polymers Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 79.4 °C | 175 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP 0123 C Polypropylene Availability: North AmericaForms: PelletsFeatures: Copolymer and Thermally ConductiveInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 79.4 °C | 175 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8006 Availability: North AmericaForms: PelletsProcessing Method: Sheet ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 79.4 °C | 175 °F | ASTM D648 |
Aaron Industries AVPP C 200-4 Virgin Polypropylene, No Break A virgin copolymer polypropylene resin specifically designed for all high speed injection molding applications, featuring excellent toughness and strength. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 79.4 °C | 175 °F | ASTM D648 |
Amco PRIMATOP PP CO 200 NB Impact Polypropylene Copolymer PP CO 200 NB is cold temperature impact resistant, heat stabilized, and nucleated. Applications include toys and consumer products.Former A-Top Polymers product; part of Amco product line since 2013.. |