Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 77.7 °C
Polymer Property :
Deflection Temperature at 0.46 MPa (66 psi) =
77.7 °C
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
77.7
°C
172
°F
Unannealed; ASTM D648
PolyOne Geon™ Vinyl Rigid Extrusion L6256 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne