Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 67.00 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 67.00 °C
152.6 °F
unannealed; ASTM D-648
Axiall Suprel® SVA 9420 Rigid PVC, Molding
Georgia Gulf Suprel® SVA 9420 Alloy is engineered for injection molding applications that require outstanding impact resistance or toughness, particularly at low temperatures. This alloy complies ..