Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 62.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 49.0 - 62.0 °C
120 - 144 °F
Average value: 56.1 °C Grade Count:36
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report..