Deflection Temperature at 0.46 MPa (66 psi) 42.0 - 57.2 °C
108 - 135 °F
Average value: 48.9 °C Grade Count:11
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi..