Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 260 - 282 °C | 500 - 540 °F | Average value: 267 °C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 250 - 282 °C | 482 - 540 °F | Average value: 275 °C Grade Count:18 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |