Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 270 °C | 518 °F | Unannealed; ASTM D648 |
PolyOne LubriOne™ SF-30GF/15T Polyphenylene Sulfide (PPS) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 270 °C | 518 °F | |
Idemitsu Kosan Xarec® WA 214 SPS, 40% Glass Filled |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 270 °C | 518 °F | |
Idemitsu Kosan Xarec® WA 214LG SPS, 40% Glass Filled Crystalline Polymer, Glass Filled |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 270 °C | 518 °F | |
Idemitsu Kosan Xarec® WA 550 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled. Used in Automotive and Industrial applications |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 270 °C | 518 °F | |
LATI Latilub 66-10T K/10 PA66, 10% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 270 °C | 518 °F | |
LATI Latiohm 57-05 PD01 G/15 PPA, 15% Glass Fiber Reinforced Semiconductive/dissipative product based on Semi-aromatic polyamide (PPA). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 270 °C | >= 518 °F | Absolute Drying; ASTM-D648 |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 270 °C | 518 °F | |
LATI Latilub 66-20T G/40 PA66, 40% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |