Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 405 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 141 - 207 °C
285 - 405 °F
Average value: 164 °C Grade Count:25
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..