Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 47.0 - 204 °C | 117 - 399 °F | Average value: 156 °C Grade Count:4 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |