Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.3 - 185 °C
209 - 365 °F
Average value: 155 °C Grade Count:7
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi..